Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00393 GPa | 0.570 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 5.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00393 GPa | 0.570 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 70A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00393 GPa | 0.570 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7100-73 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00393 GPa | 0.570 ksi | ASTM D412 |
Teknor Apex Uniprene® 73A Polyvinyl Chloride, Flexible Features: High Elastic RecoveryInformation Provided by Teknor Apex |
|||
100% Modulus | 0.00393 GPa | 0.570 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 5.0 PHR MBTS Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00393 GPa | 0.570 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 70A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00393 GPa | 0.570 ksi | ASTM D638 |
Bayshore Vinyl Compounds BVC 7200-65 Vinyl Compound BVC 7200-65 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a s.. |
|||
100% Modulus | 0.00393 GPa | 0.570 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00393 GPa | 0.570 ksi | ASTM D638 |
Colorite Polymers 5514 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |