Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00360 GPa | 0.522 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Trefsin® 3101-75 W305 Thermoplastic Rubber
(discontinued **) A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec.. |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Trefsin® 3201-75 W305 Thermoplastic Rubber
(discontinued **) A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t.. |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | DIN 53504 |
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or.. |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3470 Thermoplastic Elastomer A NSF certified, medium hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inj.. |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3470N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | ASTM D412 |
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4380 is a flame retardant, medium hardness grade processing exceptional chemical resistance, compression s.. |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ LF 6154 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | Press cure 10 Minutes @ 165°C, Ramp Post Cure in Air ASTM Die D Dumbbells |
3M Dyneon™ 301Z Translucent Perfluoroelastomer System Features and Benefits:Excellent plasma resistance with low particle count Low extractables, low outgassing, and low particle generation for ultra high purity applicationsPhosphorous-free and silica.. |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 181-73 Thermoplastic Rubber
(discontinued **) A black thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be proc.. |
|||
100% Modulus | 0.00360 GPa | 0.522 ksi | Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8500 (GLT-S) 8500 Peroxide Cured Fluoroelastomer (FKM) Formulation
(discontin FormulationViton® GLT |