Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D412 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z600P Thermoplastic Elastomer, SEBS-based, Co-injection, PA-adhesion Information provided by Polykemi AB |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | Die C; Cross direction; ASTM D412 |
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3135 can be processed by injection molding or extrusion for ap.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 400501S SBS Based Material, 50A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 500300S SEBS Based Material, Unfilled Qualities, 30A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 500350S SEBS Based Material, Unfilled Qualities, 35A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 502300S SEBS Based Material, Unfilled Qualities, 30A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 502350S SEBS Based Material, Unfilled Qualities, 35A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 502400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 502450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 602300S SEBS Based Material, Filled Qualities, 30A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 602350S SEBS Based Material, Filled Qualities, 35A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 602400S SEBS Based Material, Filled Qualities, 40A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 602450S SEBS Based Material, Filled Qualities, 45A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 602500S SEBS Based Material, Filled Qualities, 50A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 660350S SEBS Based Material, Semi-Filled Qualities, 35A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 660450S SEBS Based Material, Semi-Filled Qualities, 45A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 660500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Natural The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 662350S SEBS Based Material, Semi-Filled Qualities, 35A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Mediprene™ 660420M TPE, Medical Applications, 42A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Mediprene™ 660440M TPE, Medical Applications, 44A Hardness All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e.. |
|||
100% Modulus | 0.00100 - 0.00500 GPa | 0.145 - 0.725 ksi | ASTM D412 |
Dow Engage® Polyolefin Elastomer Engage® thermoplastic elastomers are ethylene octene copolymers produced via advanced INSITE™ catalyst and process technology, allowing control over polymer structure, properties, and rheology. .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 600400S SEBS Based Material, Filled Qualities, 40A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D412 |
3M 550 Polyurethane Adhesive Sealant Fast Cure 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D412 |
3M 560 Polyurethane Adhesive Sealant 3M™ 500-Series Polyurethane Construction Sealant, Polyurethane Sealant and Polyurethane Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. The.. |
|||
100% Modulus | >= 0.00100 GPa | >= 0.145 ksi | ASTM D412 |
3M 760 Hybrid Adhesive Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ISO 37 |
AlphaGary Evoprene™ 3276 Standard SBS Thermoplastic Elastomer Compound |
|||
100% Modulus | 0.00100 GPa | 0.145 ksi | ASTM D638 |
ELASTO UK Dryflex® 600500S SEBS Based Material, Filled Qualities, 50A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |