Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0165 GPa | 2.39 ksi | ASTM D412 |
Lubrizol Estane® 2103-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in .. |
|||
100% Modulus | 0.0165 GPa | 2.40 ksi | ASTM D412 |
ACC EP RPSP EPI Engineered Polymers Aliphatic Silicone Polymer EP RPSP Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RPSP displays extremely fa.. |
|||
100% Modulus | 0.0165 GPa | 2.40 ksi | ASTM D-638 |
Axiall 4510 Flexible PVC Non-lead stabilized 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0165 GPa | 2.39 ksi | Plasticizer conc. in vinyl film 40 phr; ASTM D638 |
BASF Palatinol® 11P-E (DUP) Linear Phthalate Formula: C30H50O4Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing .. |
|||
100% Modulus | 0.0165 GPa | 2.40 ksi | ASTM D412 |
ACC EP RP EPI Engineered Polymers Aromatic Polyurea EP RP, Aromatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RP displays extremely fast cure time.. |
|||
100% Modulus | 0.0165 GPa | 2.40 ksi | ASTM D-638 |
Axiall 1025-115A Flexible PVC Non-lead stabilized, 85C rated harness compound formulated for SAE J1128 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |