Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D412 |
Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires some load-bearing, slide abrasion, constant water contac.. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D412 |
SK Chemicals SKYTHANE® X595A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D638 |
Colorite Polymers 9204 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall H 5126A Plenum Flexible PVC Plenum-grade Cat-5(+) jacket for use over 100% FEP. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall 16930 Wire & Cable Flexible PVC Non-lead stabilized tray cable jacketing compound. UL recognized component for 720 hour sunlight resistance in black only.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall 22950 Coax & Telecom Flexible PVC Riser jacket, 25 mil over HDPE primaries.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall 35851 Moldings & Extrusions Flexible PVC 105C plug molding compound. UL recognized component for 94-5VA in all colors (3.0 mm min. thickness). UL QMFZ2 recognized component.Information provided by Georgia GulfGeorgia Gulf became Axiall C.. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall 8903 Moldings & Extrusions Flexible PVC A high quality, profile extrusion compound with excellent abrasion resistance. Especially formulated for T-moldings, tubings and other shapes where uniform flow throughout the die is required.Infor.. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall 11441 Wire & Cable Flexible PVC Clear extrusion compound formulated for applications necessitating a high degree of flame retardancy.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall 19482 Wire & Cable Flexible PVC 105°C, VW-1 rated non-lead stabilized insulation compound. Ideally suited for 18 AWG, 1/64 wall. UL approved for TW, THW, THHW applications.Information provided by Georgia GulfGeorgia Gulf became.. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall 19920 Wire & Cable Flexible PVC Non-lead stabilized 105°C insulation compound recommended for THHN-THWN circuit sizes. Well suited for 105°C; 1/64 wall in all AWG sizes. CSA approved for FT1 TWN75, TEW and AWM IA constructions.. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall 22900 Coax & Telecom Flexible PVC Riser jacket over PVC and FRPE.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall 22930 Coax & Telecom Flexible PVC Jacket compound suitable for riser applications when used with flame retardant PVC primaries. Maximum service temperature of 75°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor.. |
|||
100% Modulus | 0.0138 GPa | 2.00 ksi | ASTM D-638 |
Axiall 8424 Moldings & Extrusions Flexible PVC A clear, outdoor grade extrusion compound formulated for good UV light resistance and good low temperature properties. Recommended for fence coating applications.Information provided by Georgia Gul.. |