Mechanical Properties Metric English Comments
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D412
S&E Specialty Polymers GA-1042LF PVC
Application: UL bulletinized PVC based compound, suitable for injection molding application.Information provided by S&E Specialty Polymers
100% Modulus 0.0117 GPa
1.70 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D412
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
100% Modulus 0.0117 GPa
1.70 ksi
DIN 53504
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.0117 GPa
1.70 ksi
DIN 53504
Lubrizol ESTANE® 5715F2 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.0117 GPa
1.70 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D638
Colorite Polymers 8534 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D638
Colorite Polymers 9588 Non-Phthalate 88 Series Vinyl Compound
Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo..
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Axiall 13870 Wire & Cable Flexible PVC
Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20..
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Axiall 13872 Wire & Cable Flexible PVC
Non-lead stabilized, 720 hour sunlight resistant insulation compound recommended for TW and 75°C Class 43 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in ..
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Axiall 13880 Wire & Cable Flexible PVC
Insulation compound suitable for 75C, oil I applications. UL recognized component for TW, Oil I and 720 hour sunlight resistant applications.Information provided by Georgia GulfGeorgia Gulf became ..
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Axiall 14910 Wire & Cable Flexible PVC
Flame retardant jacket compound recommended for CM, CL2 type constructions when used over FR-PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Axiall 19910 Wire & Cable Flexible PVC
THHN-THWN, best suited for larger sizes (16 AWG and larger).Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D412
3M 5010 Polyurethane Multi-Purpose Adhesive
3M™ Polyurethane Multi-Purpose Adhesive 5010 is a one component, fast curing adhesive which forms a rigid permanent bond. 3M 5010 bonds to a wide variety of materials including wood, foam panels, f..
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Axiall 12870 Wire & Cable Flexible PVC
70°C oil, 80°C dry rated liquid tight conduit jacket meeting the requirements of UL 360.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Axiall 1055 Wire & Cable Flexible PVC
NM-B and UF-B jacket with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Axiall 19935 Wire & Cable Flexible PVC
THHN-THWN, larger sizes. Microbe resistant.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0117 GPa
1.70 ksi
ASTM D-638
Axiall 34311 Coax & Telecom Flexible PVC
CMR riser jacket over PVC or flame retardant PE insulation. Recommended for 75C applications. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorg..
100% Modulus 0.0117 GPa
1.70 ksi
ISO 37
Lubrizol ESTANE® 58141 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..