Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0108 GPa | 1.57 ksi | |
Taiwan PU Corporation TPUI-G95 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.0108 GPa | 1.57 ksi | |
Taiwan PU Corporation TPUI-L95 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.0108 GPa | 1.57 ksi | DIN 53504 |
Lubrizol ESTANE® X4985 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.0108 GPa | 1.56 ksi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 187 FT EB Thermoplastic Vulcanizate Neoplast 187 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
100% Modulus | 0.0108 GPa | 1.56 ksi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 243 HOFR Thermoplastic Vulcanizate Neoplast 243 HOFR is a flame retardant thermoplastic vulcanizate (TPV) compound, based on polyolefin chemistry, suitable for Injection Molding and Extrusion applications.RoHS Compliant, UV Stabilize.. |
|||
100% Modulus | 0.0108 GPa | 1.57 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR107-93A Seal Grade TPU Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |