Polymer Property : 100% Modulus = 0.00950 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00950 GPa
1.38 ksi
ISO/R527
Polykemi AB POLYelast TPE S902A Thermoplastic Elastomer, SBS-based
Information provided by Polykemi AB
100% Modulus 0.00950 GPa
1.38 ksi
DIN 53504
Huntsman IROGRAN® A 92 P 4207 TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
100% Modulus 0.00950 GPa
1.38 ksi
Air aged 14 days at 175°C
DuPont Vamac® GLS Sample Compound Vulcanizate Slab Cured
Test slab is press cured for 5 minutes at 177°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for thei..
100% Modulus 0.00950 GPa
1.38 ksi
ISO 37
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00950 GPa
1.38 ksi
ISO 37
Lubrizol ESTANE® GP92AB Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00950 GPa
1.38 ksi
DIN 53504
Lubrizol ESTANE® 58360 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
100% Modulus 0.00950 GPa
1.38 ksi
ISO 37
ELASTO UK Dryflex® 9012-001 TPE, Modified Injection Molding Grade for Semi Rigid Molding
The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 9012-001 is specifically designe..
100% Modulus 0.00950 GPa
1.38 ksi
ASTM D1414, ASTM D412
DuPont Performance Polymers Kalrez® 9500 Fluoroelastomer
DuPont™ Kalrez® 9500 perfluoroelastomer parts are a tan product for Deposition, Ash/Strip and Conductor (Poly/Metal) Etch processes. It has been specifically designed for use in applications where..
100% Modulus 0.00950 GPa
1.38 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR2103-90AE PTMG Polyether Polyurethane