Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00807 GPa | 1.17 ksi | ASTM D638 |
Colorite Polymers 7866 Non-Phthalate 66 Series Vinyl Compound Description: The Colorite 66 series is a family of non-toxic PVC compounds developed specifically for those medical device, food, and infant care items for which the use of a citrate* based non-phth.. |