Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00586 GPa | 0.850 ksi | STM D412 |
S&E Specialty Polymers TufGuard E™ XP-115DD-Zeta PE, Flame Retardant Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | STM D412 |
S&E Specialty Polymers TufGuard E™ XP-115D-Zeta PE, Flame Retardant Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | |
Shin-Etsu Silicones SFX-14036AU Fluorosilicone Elastomer Product Description Shincor SFX14036AU is normal 75 Durometer fluorosilicone compounds. It is designed to process well in molding applications. Product Features: Excellent fuel and solvent resistanc.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | ASTM D412 |
SK Chemicals SKYTHANE® R185A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | ASTM D638 |
Colorite Polymers 7284 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | ASTM D-638 |
Axiall 7800 Moldings & Extrusions Flexible PVC General purpose, 60°C rated molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | |
AdvanSource Biomaterials ChronoThane™ P Thermoplastic Polyurethane Elastomer AdvanSource Biomaterials Corporation manufactures and markets aromatic-based ChronoThane™ P. Some characteristics that have made it attractive to medical device manufacturers include low coefficien.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | Press Cure 10 minutes @ 177°C, Post Cure 16 hours @ 232°C |
3M Dyneon™ BRE 7231 Base Resistant Elastomer 3M™ Dyneon™ Fluoroelastomer BRE 7231 is a Base Resistant Fluoroelastomer containing 60% fluorine. It is a bisphenol cured terpolymer and is categorized as a type 4 FKM per ASTM D1418. This product.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | ASTM D-638 |
Axiall 1651 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | ASTM D-638 |
Axiall 6690 Moldings & Extrusions Flexible PVC General purpose, elastomeric vinyl compound well suited for co-extrusion with rigid PVC.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | ASTM D-638 |
Axiall 8758 Moldings & Extrusions Flexible PVC A general purpose extrusion compound recommended for extruded shapes, weatherstrips and flexible gaskets. Formulated for good UV light resistance and low temperature properties.Information provided.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2120 Fluoroelastomer 3M™ Dyneon™ Flouroelastomer FC 2120 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | ASTM D638 |
Colorite Polymers 6911X General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | ASTM D-638 |
Axiall 18752 Wire & Cable Flexible PVC Electrical grade extrusion compound with excellent low temperature performance. Maximum service temperature of 105°CInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 20.. |
|||
100% Modulus | 0.00586 GPa | 0.850 ksi | ASTM D-638 |
Axiall 83-126K Moldings & Extrusions Flexible PVC Flame retardant, 60°C rated injection molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |