Material Notes:
Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 94.0

@Time 15.0 sec
94.0

@Time 0.00417 hour
ASTM D2240
Tensile Strength 8.62 MPa
1250 psi
ASTM D412
6.896 MPa

@Temperature 100 °C,
Time 346000 sec
1000 psi

@Temperature 212 °F,
Time 96.0 hour
Oil Aged
8.3614 MPa

@Temperature 121 °C,
Time 605000 sec
1212.7 psi

@Temperature 250 °F,
Time 168 hour
Aged
Elongation at Break 500 %
500 %
ASTM D412
450 %

@Treatment Temp. 100 °C,
Time 346000 sec
450 %

@Treatment Temp. 212 °F,
Time 96.0 hour
Oil Aged
515 %

@Treatment Temp. 121 °C,
Time 605000 sec
515 %

@Treatment Temp. 250 °F,
Time 168 hour
Aged
100% Modulus 0.00586 GPa
0.850 ksi
STM D412
Thermal Properties Metric English Comments
Brittleness Temperature <= 50.0 °C
<= 122 °F
ASTM D746
Oxygen Index >= 27.0 %
>= 27.0 %
ASTM D2863