Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00465 GPa | 0.675 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00465 GPa | 0.675 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00465 GPa | 0.674 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00465 GPa | 0.675 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00465 GPa | 0.675 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00465 GPa | 0.675 ksi | ASTM D638 |
Colorite Polymers 6088 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
100% Modulus | 0.00465 GPa | 0.675 ksi | ASTM D638 |
Colorite Polymers 91-477 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00465 GPa | 0.675 ksi | ASTM D638 |
Colorite Polymers 6574 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00465 GPa | 0.674 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |