Mechanical Properties Metric English Comments
100% Modulus 0.00448 GPa
0.650 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00448 GPa
0.650 ksi
ASTM D412-97
Saint-Gobain Tygon® SE-200 Inert Tubing Formulation
Description: Tygon® SE-200: Without sacrificing the flexibility, glass-like clarity or outstanding bend radius for which Tygon® tubing is known, Tygon® Inert Tubing can handle many applic..
100% Modulus 0.00448 GPa
0.650 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00448 GPa
0.650 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N339 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00448 GPa
0.650 ksi
ASTM D638
Colorite Polymers 6500 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00448 GPa
0.650 ksi
ASTM D638
Colorite Polymers 6507 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00448 GPa
0.650 ksi
ASTM D-638
Axiall 6704 Moldings & Extrusions Flexible PVC
An expandable, low gravity, injection molding compound specifically developed for footwear applications. Finished product appearance is matte, similar to TPR.Information provided by Georgia GulfGeo..
100% Modulus 0.00448 GPa
0.650 ksi
AdvanSource Biomaterials ChronoFlex® AL 80A Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas..
100% Modulus 0.00448 GPa
0.650 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
Advanced Polymer Alloys Alcryn® 2070 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
100% Modulus 0.00448 GPa
0.650 ksi
ASTM D412
Advanced Polymer Alloys Alcryn® 2180 NC Melt Processable Rubber
Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades..
100% Modulus 0.00448 GPa
0.650 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2110Q Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FC 2110Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..
100% Modulus 0.00448 GPa
0.650 ksi
ASTM D-638
Axiall 10640 Wire & Cable Flexible PVC
Non-lead stabilized general purpose, highly flexible jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00448 GPa
0.650 ksi
ASTM D-638
Axiall 10641 Wire & Cable Flexible PVC
Non-lead stabilized general purpose jacket compound designed for good flexibility and good low temperature performance.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2..
100% Modulus 0.00448 GPa
0.650 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 45 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Copyright © lookpolymers.com All Rights Reserved