Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00314 GPa | 0.456 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TCP Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00314 GPa | 0.455 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 285ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00314 GPa | 0.455 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 285ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
100% Modulus | 0.00314 GPa | 0.455 ksi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 155 FT EB Thermoplastic Vulcanizate Neoplast 155 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, .. |
|||
100% Modulus | 0.00314 GPa | 0.456 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR TCP Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00314 GPa | 0.455 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00314 GPa | 0.455 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |