Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00290 GPa | 0.421 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z700 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
100% Modulus | 0.00290 GPa | 0.420 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Plasthall 7050 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00290 GPa | 0.421 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap.. |
|||
100% Modulus | 0.00290 GPa | 0.421 ksi | ASTM D412 |
UBE UBEPOL BR153A Oil-Extended BR Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
100% Modulus | 0.00290 GPa | 0.421 ksi | ASTM D412 |
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
100% Modulus | 0.00290 GPa | 0.421 ksi | ASTM D412 |
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
100% Modulus | 0.00290 GPa | 0.420 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00290 GPa | 0.420 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 10.0 PHR Plasthall 7050 Plasticizer Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00290 GPa | 0.421 ksi | JIS 6251 (Dumbbells) |
DuPont Performance Polymers Kalrez® 8002 FFKM Perfluoroelastomer Kalrez® 8002 is a specialty compound targeted specifically for select semiconductor plasma and gas deposition applications. This clear, unfilled compound offers very low particle generation in oxyg.. |
|||
100% Modulus | 0.00290 GPa | 0.420 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR MBT Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00290 GPa | 0.421 ksi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |