Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00234 GPa | 0.340 ksi | ASTM D412 |
Lubrizol Estane® AG 4950 Thermoplastic Polyurethane Type: Estane® AG 4950 is a polyether based aliphatic thermoplastic polyurethane (TPU) specifically formulated to be used as an adhesive interlayer in transparencies for electronic displays, aerospa.. |
|||
100% Modulus | 0.00234 GPa | 0.339 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 70A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
100% Modulus | 0.00234 GPa | 0.340 ksi | ASTM D 412 |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
100% Modulus | 0.00234 GPa | 0.340 ksi | Press Cure 7 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FT 2430 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FT 2430 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
100% Modulus | 0.00234 GPa | 0.339 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 70A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |