Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 100 J @Thickness 4.00 mm |
73.8 ft-lb @Thickness 0.157 in |
Multi-axial, total energy; ISO 6603-2 |
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This.. |