Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 8.00 J @Temperature -30.0 °C |
5.90 ft-lb @Temperature -22.0 °F |
Multi-Axial Impact, Fractovis J; Energy Peak; ASTM-D3763 |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |
|||
Impact Test | 8.00 J @Temperature -20.0 °C |
5.90 ft-lb @Temperature -4.00 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Ultem EXUM0169 PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Impact Test | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA 30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Verton RV004ESV_GY7E070 PA 66 Preliminary data for 20% long glass fiber filled, single pellet color gray, PA66This data was supplied by SABIC-IP for the Americas region. |