Polymer Property : Impact Test = 45.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 61.0 J

@Temperature 23.0 °C
45.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS
AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Americas region.
Impact Test 61.0 J

@Temperature 23.0 °C
45.0 ft-lb

@Temperature 73.4 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Cycoloy® MC9000 PC+ABS (Asia Pacific)
AUTOMOTIVE. PC+ABS; high heat resistant. Ductile at room temperature. Excellent flow.This data was supplied by SABIC-IP for the Asia Pacific region.
Impact Test 61.0 J

@Temperature -30.0 °C
45.0 ft-lb

@Temperature -22.0 °F
Instrumented Impact Total Energy; ASTM D 3763
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East)
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.