Polymer Property : Impact Test = 22.9 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 31.0 J

@Temperature 23.0 °C
22.9 ft-lb

@Temperature 73.4 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin
50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS
Impact Test 31.0 J

@Temperature -40.0 °C
22.9 ft-lb

@Temperature -40.0 °F
Instrumented Impact Energy @ peak; ASTM D 3763
SABIC Innovative Plastics Noryl GTX GTX904 PPE+PS+PA
Unreinforced; improved processing; excellent chemical resistance; 320F (160C) HDT.This data was supplied by SABIC-IP for the Americas region.
Impact Test 31.0 J

@Temperature 23.0 °C
22.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® 835 Sheet Extrusion Grade
Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex ..
Impact Test 31.0 J

@Thickness 102 mm
22.9 ft-lb

@Thickness 4.00 in
Multi-axial, at failure; ASTM D3763
Azdel Plus C507-B01 50% Chopped Fiber Mat / PP Resin Matrix (Mineral filled)
AZDEL® C507-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu..
Impact Test 31.0 J

@Thickness 4.00 mm
22.9 ft-lb

@Thickness 0.157 in
Multi-axial, at failure; ASTM D3763
Azdel Plus R451-B02 45% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R451-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr..