Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | >= 22.6 J @Thickness 5.99 mm, Temperature 22.8 °C |
>= 16.7 ft-lb @Thickness 0.236 in, Temperature 73.0 °F |
Drop Ball Impact Test, 1 inch dart |
Plaskolite Mustang PETG Sheet MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy.. |
|||
Impact Test | >= 22.6 J @Thickness 5.99 mm, Temperature -17.8 °C |
>= 16.7 ft-lb @Thickness 0.236 in, Temperature 0.000 °F |
Drop Ball Impact Test, 1 inch dart |
Plaskolite Mustang PETG Sheet MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cy.. |
|||
Impact Test | 22.6 J @Temperature -40.0 °C |
16.7 ft-lb @Temperature -40.0 °F |
At Yield. Deflection: 693 mils, Force: 425 lbs (Instrumented Impact, 9000 in/min) |
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Impact Test | 22.6 J @Temperature -40.0 °C |
16.7 ft-lb @Temperature -40.0 °F |
At Yield. Deflection: 693 mils, Force: 425 lbs (Instrumented Impact, 9000 in/min) |
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer Information provided by Teknor Apex Company |