Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 20.3 J @Temperature 23.0 °C |
15.0 ft-lb @Temperature 73.4 °F |
Instrument Impact, Total Energy; ASTM D3763 |
ExxonMobil OPTEMA™ TC 115 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 115 is an ethylene methyl acrylate copolymer, which can be used as a compatibilizer and impact modifier for engineering thermoplastics. It has been processed at temperatures up to 625°F w.. |
|||
Impact Test | 20.3 J @Temperature -40.0 °C |
15.0 ft-lb @Temperature -40.0 °F |
Instrumented Impact, Total Energy; ASTM D3763 |
ExxonMobil OPTEMA™ TC 220 Molding Ethylene Methyl Acrylate OPTEMA TC 220 is an ethylene methyl acrylate copolymer, which can be used in specialty bonding applications and as a toughener for engineering polymers. It can been processed at temperatures as low .. |
|||
Impact Test | 20.4 J @Temperature 23.0 °C |
15.0 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (10 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Impact Test | 20.3 J @Temperature 23.0 °C |
15.0 ft-lb @Temperature 73.4 °F |
Multi-axial, at failure, measured on flat plaques; ASTM D3763 |
Azdel SuperLite® SL552000-100 PP Resin Matrix / 55% Glass Fiber (12 mm Molded Thickness) AZDEL SuperLite® SL552000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |