Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Peak Energy; ASTM-D3763 |
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin 50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS |
|||
Impact Test | 31.0 J @Temperature -40.0 °C |
22.9 ft-lb @Temperature -40.0 °F |
Instrumented Impact Energy @ peak; ASTM D 3763 |
SABIC Innovative Plastics Noryl GTX GTX904 PPE+PS+PA Unreinforced; improved processing; excellent chemical resistance; 320F (160C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Impact Test | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Diamond Polymers Centrex® 835 Sheet Extrusion Grade Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex .. |
|||
Impact Test | 31.0 J @Thickness 102 mm |
22.9 ft-lb @Thickness 4.00 in |
Multi-axial, at failure; ASTM D3763 |
Azdel Plus C507-B01 50% Chopped Fiber Mat / PP Resin Matrix (Mineral filled) AZDEL® C507-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat and mineral filler contained within a polypropylene resin matrix. This composite material featu.. |
|||
Impact Test | 31.0 J @Thickness 4.00 mm |
22.9 ft-lb @Thickness 0.157 in |
Multi-axial, at failure; ASTM D3763 |
Azdel Plus R451-B02 45% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R451-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr.. |