Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Impact Test = 30.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Total Energy; ASTM-D3763
Ineos ABS Lustran® 256 Extrusion Blending Grade
Lustran® ABS 256 resin is a natural, medium-flow, medium-impact, low-gloss, low-gel extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It is used for blending with other Lustran® ABS vi..
Impact Test 30.0 J

@Temperature -18.0 °C
22.1 ft-lb

@Temperature -0.400 °F
Multiaxial Impact (3.4 m/s, 40-mm ring, M831 Striker); Total Energy; ASTM-D3763
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade
Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components.
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
Instrumented Impact (0.5-in. dart, 3-in. clamp, 7.6 mph); Total Energy; ASTM-D3763
Ineos ABS Lustran® LK197 ABS, Extrusion Grade
Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e..
Impact Test 30.0 J

@Temperature -30.0 °C
22.1 ft-lb

@Temperature -22.0 °F
ASTM D3763
Diamond Polymers Centrex® 833 Sheet Extrusion Grade
Centrex 833 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it ..
Impact Test 30.0 J

@Temperature -18.0 °C
22.1 ft-lb

@Temperature -0.400 °F
ASTM D3763
Diamond Polymers Centrex® 835 Sheet Extrusion Grade
Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex ..
Impact Test 30.0 J

@Temperature 23.0 °C
22.1 ft-lb

@Temperature 73.4 °F
ASTM D3763
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade
Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high..
Impact Test 30.0 J

@Thickness 4.00 mm
22.1 ft-lb

@Thickness 0.157 in
Multi-axial, total energy; ISO 6603-2
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia..
Impact Test 30.0 J

@Thickness 4.00 mm
22.1 ft-lb

@Thickness 0.157 in
Multi-axial, total energy; ISO 6603-2
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Impact Test 30.0 J

@Diameter 25.4 mm,
Temperature 20.0 °C
22.1 ft-lb

@Diameter 1.00 in,
Temperature 68.0 °F
310 HB
Assab Steels 718HH Plastic Mold Material
IMPAX SUPREME is a premium-quality vacuum-degassed Cr-Ni-Mo-alloyed steel which is supplied in the hardened and tempered condition. IMPAX SUPREME is manufactured to consistently high quality standar..