Polymer Property : Izod Impact Unnotched = 14.9 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 14.9 J
11.0 ft-lb
Oil Quenched at 1238°C; 510°C Temper Temperature
Latrobe Dynavanâ„¢ ASTM T15 Super High Speed Steel
DYNAVAN (T15) is a super high speed steel designed for extra-high wear resistance and superior hot hardness. These properties result from the high carbon and vanadium contents which produce numerous..
Izod Impact Unnotched 14.9 - 31.2 J
11.0 - 23.0 ft-lb
Carpenter Micro-Melt® M-42 Alloy (AISI M42)
Micro-Melt® M-42 alloy is a powder metal super-high-speed steel possessing a hardness capability of Rockwell C 68/70. This alloy has been used for cutting tools in the toughest machining operations..
Izod Impact Unnotched 14.9 J
11.0 ft-lb
ASTM D256
Solvay Specialty Polymers Xydar® M-345 Liquid Crystal Polymer, 45% Mineral Filled  (discontinued **)
XYDAR M-345 Liquid Crystal Polymer (LCP) is a 45% mineral-filled injection molding grade with exceptional moldability. XYDAR M-345 resin can fill very thin walls over long flow lengths with little o..