Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 40.0 MPa | 5800 psi | 10% Def.; ASTM D695 |
Quadrant EPP Ketron® LSG PEEK-CLASSIX Biocompatibility tested (ASTM Product Data Sheet) KETRON® PEEK-CLASSIX LSG white stock shapes are produced from Invibio® PEEK-CLASSIX White resin. This material exhibits a unique combination of mechanical properties, temperature and chemical re.. |
|||
Compressive Strength | 40.0 MPa @Time 3.60e+7 sec |
5800 psi @Time 10000 hour |
|
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Compressive Strength | 40.0 MPa | 5800 psi | ASTM-C773 |
CoorsTek PolyGlyde™ 2000 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
Compressive Strength | 40.0 MPa | 5800 psi | Cold Crushing Strength |
Chosun Refractories A12HM Magnesia Carbon Bricks for Electric Arc Furnace Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 40.0 MPa | 5800 psi | Cold Crushing Strength |
Chosun Refractories A12S Magnesia Carbon Bricks for Electric Arc Furnace Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 40.0 MPa | 5800 psi | Cold Crushing Strength |
Chosun Refractories C15A Magnesia Carbon Brick for Converter Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | >= 40.0 MPa | >= 5800 psi | Axial; IEC 1212-2 4.2 |
Hippe SI GC 21 Woven Glass Cloth Reinforced Silicone Resin - Round, Rolled Tube Good mechanical, electrical and electronic applications when exposed to high relative humidity.Information provided by Hippe. |
|||
Compressive Strength | 40.0 MPa | 5800 psi | Cold Crushing Strength |
Chosun Refractories L12H Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 40.0 MPa | 5800 psi | Cold Crushing Strength |
Chosun Refractories L12HU Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 40.0 MPa | 5800 psi | Cold Crushing Strength |
Chosun Refractories L12S Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 40.0 MPa | 5800 psi | Cold Crushing Strength |
Chosun Refractories L15H Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 40.0 MPa | 5800 psi | Cold Crushing Strength |
Chosun Refractories L15HU Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 40.0 MPa | 5800 psi | Cold Crushing Strength |
Chosun Refractories L15S Magnesia Carbon Bricks for Ladle Slag Line Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | >= 40.0 MPa | >= 5800 psi | Ambient |
China-Yixing Longly Refractories ASM-130 Cordierite-Mullite Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b.. |
|||
Compressive Strength | 40.0 MPa | 5800 psi | Cold Crushing Strength |
Chosun Refractories A12H Magnesia Carbon Bricks for Electric Arc Furnace Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |