Mechanical Properties Metric English Comments
Compressive Strength 37.0 MPa

@Time 360000 sec
5370 psi

@Time 100 hour
Wolf Kunststoff ZEDEX® ZX-530 A5D Polymer Alloy
Main Characteristics: Low Creep; Low moisture absorption; Flame retardant; Low impurity ions; Good machinability; FDA compliant LABS; Extremely low outgassing; Less expensive than PEEK; Stress resis..
Compressive Strength >= 37.0 MPa
>= 5370 psi
Ambient
China-Yixing Longly Refractories ASM-125 Cordierite-Mullite
Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b..