Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 3.50 MPa | 508 psi | EN 1094-5: 1995 |
Skamol Group Moler SM-65 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Compressive Strength | 3.50 MPa | 508 psi | perpendicular to plane; ISO 844 |
3A Composites Core Materials AIREX® T90.210 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has good mechanical properties and resistance to fatigue, is chemic.. |
|||
Compressive Strength | 3.50 MPa | 508 psi | average; perpendicular to plane; ISO 844 |
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r.. |