Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 293 MPa | 42500 psi | ISO 604 |
Vyncolit BXE7665 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Excellent electrical properties combined with very good mechanical properties. Grade especially suitable for electrical applications.Information pro.. |
|||
Compressive Strength | 293 MPa | 42500 psi | ISO 604 |
Vyncolit BXE7670 Glass Filled Phenolic Molding Compound Novolac resin based, mainly glass fiber filled. Due to its unique composition, excellent balance between mechanical, thermal and dimensional stability.Information provided by Sumitomo Bak North Ame.. |