Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.276 - 0.345 MPa | 40.0 - 50.0 psi | Cold Crush Strength |
Unifrax Foamfrax® Isofoam® RG Insulation Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory.. |
|||
Compressive Strength | 0.276 - 0.345 MPa | 40.0 - 50.0 psi | Cold Crush Strength |
Unifrax Foamfrax® RG Insulation Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory.. |
|||
Compressive Strength | 0.276 - 0.345 MPa | 40.0 - 50.0 psi | Cold Crush Strength |
Unifrax Foamfrax® RG Plus Insulation Like Foamfrax RG, Foamfrax® RG Plus combines refractory ceramic fiber, refractory cement, and a high-temperature binder solution that can be combined in the field using the uniqued Foamfrax process.. |
|||
Compressive Strength | 0.276 MPa | 40.0 psi | 5% Deformation; Green |
Unifrax Fiberfrax® Duraboard® 350ES Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |
|||
Compressive Strength | 0.276 MPa | 40.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ E1515 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Compressive Strength | 0.276 MPa | 40.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ E1520 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Compressive Strength | 0.276 MPa | 40.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ E1840 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Compressive Strength | 0.276 MPa | 40.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ E1840H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Compressive Strength | 0.276 MPa | 40.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ E1860 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Compressive Strength | 0.276 MPa | 40.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ E1860H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |