Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 148 MPa | 21500 psi | 10% Def.; ASTM D695 |
Quadrant EPP Techtron® 1000 PPS Extruded Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Compressive Strength | 148 MPa | 21500 psi | |
Poco Graphite EDM-4 EDM Graphite POCO's EDM-4 is our premier offering in the Ultrafine classification. This highly isotropic grade combines strength with moderate hardness, yielding superior electrode fabrication characteristics. T.. |
|||
Compressive Strength | 148 MPa | 21500 psi | |
SGL Carbon Group EK 10 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 148 MPa | 21500 psi | |
SGL Carbon Group EK 17 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 148 MPa | 21500 psi | |
SGL Carbon Group EK 2239 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 148 MPa | 21500 psi | |
SGL Carbon Group V 1626 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 148 MPa | 21500 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Compressive Strength | 148 MPa | 21500 psi | ASTM D695 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Compressive Strength | 148 MPa | 21500 psi | |
Cosmic Plastics ID-40 Orlon Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 148 MPa | 21500 psi | Ultimate; TM R050-38 |
Resinlab® EP965SC-7 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Compressive Strength | 148 MPa | 21500 psi | Break; TM R050-38 |
Resinlab® EP965SC-7 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Compressive Strength | 148 MPa | 21500 psi | Ultimate; TM R050-38 |
Resinlab® EP965SC-7 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Compressive Strength | 148 MPa | 21500 psi | Break; TM R050-38 |
Resinlab® EP965SC-7 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965SC-7 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett.. |
|||
Compressive Strength | 148 MPa | 21500 psi | ASTM D695 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |