Polymer Property : Compressive Strength = 8.50 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 6.50 - 8.50 MPa

@Temperature 23.0 °C,
Time 86400 sec
943 - 1230 psi

@Temperature 73.4 °F,
Time 24.0 hour
@ 1% deformation, 140 Kg/cm<sup>2</sup>; ASTM D621
Adamas Adalon® 403 PTFE, 15% Polyimide
Information provided by Adamas, HPM