Compressive Strength 110 - 130 MPa
16000 - 18900 psi
GB/T 1040
Beijing Evergrow Resources Glass Filled Nylon
Information provided by Beijing Evergrow Resources.
Compressive Strength 110 - 130 MPa
16000 - 18900 psi
ISO 604
Vyncolit 3520 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..