Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 95.1 - 123 MPa | 13800 - 17800 psi | |
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific .. |