Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 93.2 MPa | 13500 psi | ISO 604 |
Polikim KESTAMID® PA6G Polyamide 6 Kestamid® is also known as Cast Polyamide or Cast Nylon. Kestamid® is an engineering plastic used commonly in all industrial branches for its superior mechanical, physical, chemical and electrical.. |
|||
Compressive Strength | 93.2 MPa | 13500 psi | ISO 604 |
Polikim KESTLUB® Polyamide 6 + Lubricant Kestlub® is a special type of cast polyamide ideal for bearings. It is produced by adding lubricants to cast polyamide through special processes. It performs extremely well in bearing applications .. |
|||
Compressive Strength | 93.2 MPa | 13500 psi | ISO 604 |
Polikim KESTOIL® Polyamide 6 + Lubricant Kestoil® is a self-lubricated, strong, wear resistant engineering plastic with a low coefficient of friction. Implicit in its nature, it has many properties that no other material has in combinatio.. |
|||
Compressive Strength | 93.2 MPa | 13500 psi | ISO 604 |
Polikim KESTAMID® GRF Polyamide 6, Graphite Filled Graphite and special lubricants are evenly dispersed in its entirety in this type of Polikim's cast polyamide. The material is dark grey colored. Kestamid®-GRF has a high degree of crystallinity an.. |
|||
Compressive Strength | 93.2 MPa | 13500 psi | Cold Crushing |
Sharadaa Ceramics PCF90 (L) Precast Prefired Brick Features: Manufactured under controlled conditions under refractory engineers supervision; Measured Quantity/Temperature of water, mixing by Intensive counter current mixers, Forming by Vibro Castin.. |
|||
Compressive Strength | 93.2 MPa | 13500 psi | ISO 604 |
Polikim KESTAMID® HS Polyamide 6, Heat Resistant Kestamid-HS® is Polikim’s cast polyamide with increased heat resistance. Thermal stabilizer additives increase thermal aging significantly. In operating temperatures over 80°C, it performs with .. |