Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 92.05 MPa | 13350 psi | |
CMT Materials HYTAC® FLX Good Durability, Easily Machined & Polished Copolymer Syntactic HYTAC-FLX has been improved for optimum performance in transparent applications. The enhanced formulation is easy to polish and results in minimal to no scratches with transparent sheet materials. .. |
|||
Compressive Strength | 92.05 MPa | 13350 psi | ultimate load |
BNZ Materials Transite 1000 Low Temperature Industrial Board These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry ind.. |