Compressive Strength |
850 MPa |
123000 psi |
|
Sapco C 221 Steatite
Information provided by Sapco. |
Compressive Strength |
>= 850 MPa |
>= 123000 psi |
Chemically Strengthened to >50 µm Depth |
Corning Gorilla® Glass 4 Touch Screen Glass
Gorilla® Glass 4 is just as thin and light as previous versions of Gorilla® Glass, but has been formulated to deliver dramatically improved damage resistance allowing improved in-field performance.. |
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-28EH Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-28UH Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-30EH Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-35 Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-35H Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-35M Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-35UH Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-38 Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-38SH Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-40SH Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-42 Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-42SH Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-44H Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-45M Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-50 Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-30EZ Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-33H Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-33SH Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-33UH Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-38H Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-38M Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-40 Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-42H Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-33M Neodymium Iron Boron Magnetic Material
|
Compressive Strength |
850 - 1050 MPa |
123000 - 152000 psi |
|
Alliance N-48 Neodymium Iron Boron Magnetic Material
|