Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 6.50 - 9.50 MPa | 943 - 1380 psi | Cold Crushing Strength |
Gouda Vuurvast GI 34 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 6.50 - 8.50 MPa @Temperature 23.0 °C, Time 86400 sec |
943 - 1230 psi @Temperature 73.4 °F, Time 24.0 hour |
@ 1% deformation, 140 Kg/cm<sup>2</sup>; ASTM D621 |
Adamas Adalon® 403 PTFE, 15% Polyimide Information provided by Adamas, HPM |