Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 48.3 MPa | 7000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Fluorosint® 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers (ASTM Product Data Sheet) Chemical resistance parallels PTFE Continuous use temperatures to 500°F (260°C) Compared to PTFE higher load carrying capability 1/9 of the deformation under load lower coefficient of thermal exp.. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | ASTM D695 |
ScanTube ECTFE Tubing Information provided by ScanTube, Inc. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | ASTM D695 |
ScanTube ETFE Tubing Information provided by ScanTube, Inc. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | ASTM-C773 |
CoorsTek PolyGlyde™ 5400 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | |
Cotronics Resbond™ 903HP High Temperature Ceramic Adhesive, Hi-Bond Strength |
|||
Compressive Strength | 48.3 - 207 MPa | 7000 - 30000 psi | |
Du-Co Ceramics S-470 Aluminum Silicate Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Compressive Strength | 48.3 - 207 MPa | 7000 - 30000 psi | |
Du-Co Ceramics S-699 Alumina Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Compressive Strength | 48.3 - 51.7 MPa | 7010 - 7500 psi | ASTM C133 |
Ceradyne Thermo-Sil® HS Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | |
Aremco Ceramacast™ 645-N High Temperature Potting & Casting Material Silica Castable ceramic with low thermal conductivity. |
|||
Compressive Strength | 48.3 - 55.2 MPa | 7000 - 8000 psi | |
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Compressive Strength | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Compressive Strength | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Abatron AboCast 7802-1/AboCure 7804-4 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | Break; TM R050-38 |
Resinlab® EP1296 Highly Filled, Moderately Thixotropic Black Casting Resin Resinlab™ EP1296 is a highly filled, moderately thixotropic black casting resin designed for applications requiring good thermal conductivity, low shrinkage and a low CTE. It was especially formula.. |
|||
Compressive Strength | 48.3 - 51.7 MPa | 7010 - 7500 psi | ASTM C133 |
Ceradyne Thermo-Sil® Castable 220 Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |