Mechanical Properties Metric English Comments
Compressive Strength 2200 MPa
319000 psi
DIN 51067T1
CeramTec MZ 111 HIP Zirconia, ZrO2-Y2O3
MZ 111 HIP is a yttria-stabilized tetragonal zirconia ceramic.
Compressive Strength 2200 MPa
319000 psi
DIN 51067T1
CeramTec MZ 111 Zirconia, ZrO2-Y2O3
MZ 111 is a yttria-stabilized tetragonal zirconia used in dental applications.
Compressive Strength 2200 MPa
319000 psi
DIN 51067T1
CeramTec MZ 429 Zirconia, ZrO2-Y2O3
MZ 429 is a yttria-stabilized zirconia ceramic.
Compressive Strength 2200 MPa
319000 psi
DIN 51067T1
CeramTec Rocar® ST Silicon Carbide, SSiC
Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat..
Compressive Strength 2200 MPa
319000 psi
Rc0.2; at HRC=58
Bohler-Uddeholm UDDEHOLM Vancron 40 nitrided powder tool steel
Description: Uddeholm Vancron 40 is a nitrided powder tool steel, which means that a “surface coating” is already integrated into the finished tooling material. The result is a tool surface with v..
Compressive Strength 2200 MPa
319000 psi
HRC 62 R<sub>c</sub>0.2.
Assab Steels ASSAB XW-41 Cold Work Steel
XW-41 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength Good through-hardening propertiesHigh stability i..
Compressive Strength 2200 MPa
319000 psi
HRC 62 R<sub>p</sub>0.2
Assab Steels ASSAB XW-42 Cold Work Steel
XW-42 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength High hardness after hardeningGood through-hardeni..