Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 215 MPa | 31200 psi | ASTM D695 |
Premix Premi-Glas® 1200-30 Polyester SMC Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac.. |
|||
Compressive Strength | 215 MPa | 31200 psi | ASTM D695 |
Premix Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Compressive Strength | 215 MPa | 31200 psi | ASTM D695 |
Glastic Laminates/Shapes 1580 Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3. Developed to meet the television industry's safety assurance requirements. |
|||
Compressive Strength | 215 MPa | 31200 psi | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP LC008EXQ PEEK LNP* THERMOCOMP* LC008EXQ is a compound based on Polyetheretherketone containing 40% Carbon Fiber. Added features of this grade include: Electrically Conductive, Easy Molding. |
|||
Compressive Strength | 215 MPa | 31200 psi | ASTM D695 |
Plenco 2567 Phenolic, Granular, Compression Molded PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo.. |
|||
Compressive Strength | 215 MPa | 31200 psi | ASTM D695 |
Plenco 5482 Phenolic, Granular, Transfer Molded PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect.. |
|||
Compressive Strength | 215 MPa | 31200 psi | ASTM D695 |
Plenco 6015 Phenolic, Briquette, Transfer Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Compressive Strength | 215 MPa | 31200 psi | ASTM D695 |
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent fle.. |
|||
Compressive Strength | 215 MPa | 31200 psi | |
Abatron AboCast 8504-1 One-Component Epoxy AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications. |
|||
Compressive Strength | 215 MPa | 31200 psi | ISO 604 |
Sumitomo Bakelite North America RX® 852 Novolac Phenolic Fiberglass reinforced phenolic novolac compound with good dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |