Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 214 MPa | 31000 psi | ASTM D695 |
Sumitomo Bakelite Durez® 31906 Phenolic, Compression Grade Durez 31906 Black Phenolic is an asbestos free, medium impact, molding compound. It is designed for applications where additional mechanical strength is required.Information provided by Sumitomo Ba.. |
|||
Compressive Strength | 214 MPa | 31000 psi | ASTM D695 |
Saint-Gobain Meldin® 5320 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Compressive Strength | 214 MPa | 31000 psi | ASTM D695 |
Plenco 6500 Phenolic, Briquette, Injection Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Compressive Strength | 214 MPa | 31000 psi | ASTM D695 |
Plenco 2000 Phenolic, Granular, Transfer Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Compressive Strength | 214 MPa | 31000 psi | ASTM D695 |
PolyOne Edgetek® PI-40GF/000 Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |