Mechanical Properties Metric English Comments
Compressive Strength 2.00 MPa
290 psi
EN 1094-5: 1995
Skamol Group ISOPERLOR 550P Perlite Insulating Brick & Block
ISOPERLOR perlite insulating bricks & blocks have the following characteristics: Max. service temperature 900°C (1652°F)Back-up insulation onlyExcellent insulating propertiesVery lightweight a..
Compressive Strength 2.00 MPa
290 psi
Cold
Unifrax Excelfrax® 1900 Panel Microporous Insulation
Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo..
Compressive Strength 2.00 MPa
290 psi
Lower Yield in the Through Plane Direction
Cymat A35620SC 040SS Stabilized Aluminum Foam
Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it ..
Compressive Strength 2.00 MPa
290 psi
Cold Crush Strength; ASTM C133
BNZ Materials BNZ-26-60 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Compressive Strength 2.00 MPa
290 psi
Cold Crush Strength; ASTM C133
BNZ Materials BNZP-23 Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Compressive Strength 2.00 MPa
290 psi
Cold Crush Strength; ASTM C133
BNZ Materials BNZP-23B Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Compressive Strength 2.00 MPa
290 psi
Cold Crush Strength; ASTM C133
BNZ Materials BNZP-25L Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Compressive Strength 2.00 MPa

@Temperature 200 °C
290 psi

@Temperature 392 °F
ISO 604
Brandenburger BL 70 Slide Bearing Material
BL 70 is a low friction material that exhibits stability at high temperatures. Its applications include high-load low friction tracks and linings in transport and conveying systems, high-stressed b..
Compressive Strength 2.00 MPa
290 psi
average; perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Compressive Strength 2.00 MPa
290 psi
average; perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® T90.150 Easy Processing Structural FST Foam