Polymer Property : Compressive Strength = 180 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 180 MPa
26100 psi
Test specimen flat tested; ISO 604
Hexion Bakelite™ PF 6507 Phenolic Formaldehyde Resin, Elasticized, Low Shrinkage, Resistant to High Temperatures, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, elastomer modified, galvanizable, heat resistant, good media resistance, high dimensional stability at raised temperature, hi..
Compressive Strength 180 MPa
26100 psi
ASTM D695
Sumitomo Bakelite North America Epiall® 1908B-1 Short Glass Fiber Reinforced Epoxy
Epiall 1908B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided ..
Compressive Strength 180 - 220 MPa
26100 - 31900 psi
ISO 604
Vyncolit G885 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group
Compressive Strength 180 MPa
26100 psi
Absolute Drying; ASTM-D695
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Compressive Strength 180 MPa
26100 psi
ASTM D695
Plenco 3597 Phenolic, Granular, Injection Molded
PLENCO 03597 is a mineral filled phenolic molding compound offering excellent flammability ratings even at thin cross sections, along with excellent arc and comparative track resistance values. UL r..
Compressive Strength 180 MPa
26100 psi
ASTM D695
Plenco 6301 Phenolic, Granular, Injection Molded
PLENCO 06301 is an inorganic reinforced phenolic molding compound, offering excellent heat resistance, dimensional stability, and processability as required for typical automotive applications. It i..
Compressive Strength 180 MPa

@Temperature 23.0 °C,
Time 86400 sec
26100 psi

@Temperature 73.4 °F,
Time 24.0 hour
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Tubes
Description: Mechanical and electrical applications. Arc-resistant and tracking-resistant material. Good flame resistance. Self-extinguishing. Halogen-free. Lower high-voltage values and insulation ..
Compressive Strength 180 MPa

@Treatment Temp. 150 °C,
Time 3600 sec
26100 psi

@Treatment Temp. 302 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m..
Compressive Strength 180 MPa

@Treatment Temp. 200 °C,
Time 3600 sec
26100 psi

@Treatment Temp. 392 °F,
Time 1.00 hour
ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets
Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope..
Compressive Strength 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT 1031 Polyimide, 40% Graphite Filled (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Compressive Strength 180 MPa

@Temperature 23.0 °C
26100 psi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Compressive Strength 180 MPa

@Temperature 23.0 °C,
Time 86400 sec
26100 psi

@Temperature 73.4 °F,
Time 24.0 hour
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2
Elektro-Isola Etronax MF G Phenolic, Cotton Fabric Reinforcement, Black, Tubes
Description: Mechanical applications. Impact-resistant, noise-reducing, wear-resistant material. Well suited as a low-friction material. High wear resistance in aggressive and dust-filled environmen..
Compressive Strength >= 180 MPa
>= 26100 psi
ISO 604
Bulk Molding Compounds tetra-DUR F 4209 Bulk Molding Compound
Highest Arc resistanceTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), therm..
Compressive Strength >= 180 MPa
>= 26100 psi
ISO 604
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound
Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat..