Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 164 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 164 MPa
23800 psi
ASTM D695
Glastic BMC SLC-1000 Glass-Reinforced Polyester
Data provided by Glastic Corporation.Medium strength, V-0, adjustable shrinkage.
Compressive Strength 164 MPa
23800 psi
ASTM D695
Plenco 3356 Phenolic, Granular, Compression Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..
Compressive Strength 164 MPa

@Temperature 23.0 °C
23800 psi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT™ 2061 Polyimide, 15% Graphite, 10% PTFE Filled (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Compressive Strength 164 MPa
23800 psi
ASTM D695
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Compressive Strength 164 MPa
23800 psi
10% Def.; ASTM D695
Quadrant EPP Semitron® ESd 420- CM Dissipative Polyetherimide(ASTM Product Data Sheet)