Polymer Property : Compressive Strength = 1380 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1380 MPa
200000 psi
Meehanite AQ Flake Graphite Cast Iron
Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treate..
Compressive Strength 1380 MPa
200000 psi
Meehanite GM-60 Flake Graphite Cast Iron
Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a..