Mechanical Properties Metric English Comments
Compressive Strength 11.0 MPa
1600 psi
EN 1094-5: 1995
Skamol Group VIP 12 Vermiculite Insulating Slab
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr..
Compressive Strength >= 11.0 MPa
>= 1600 psi
Engineered Syntactic Systems SF-22 Subsea Macrosphere Syntactic Void Filler
In applications where density is critical, the four part SF-22 kit is used. This system utilizes fiber reinforced epoxy macrospheres in combination with the standard microsphere syntactic to provide..
Compressive Strength 11.0 MPa
1600 psi
Elastic Limit
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy
Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor..
Compressive Strength 11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
1% deformation; ASTM D695
Daikin NEOFLON EA-LR43 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Compressive Strength 11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
1% deformation; ASTM D695
Daikin NEOFLON EP-521 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Compressive Strength 11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
1% deformation; ASTM D695
Daikin NEOFLON EP-610 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Compressive Strength 11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
1% deformation; ASTM D695
Daikin NEOFLON EP-610AS ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Compressive Strength 11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
1% deformation; ASTM D695
Daikin NEOFLON RP-4020 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Compressive Strength 11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
1% deformation; ASTM D695
Daikin NEOFLON RP-4040 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Compressive Strength 11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
1% deformation; ASTM D695
Daikin NEOFLON RP-5000 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Compressive Strength 11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
1% deformation; ASTM D695
Daikin NEOFLON RP-5000AS EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Compressive Strength 11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
1% deformation; ASTM D695
Daikin NEOFLON EP-620 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Compressive Strength 11.0 MPa

@Temperature 25.0 °C
1600 psi

@Temperature 77.0 °F
1% deformation; ASTM D695
Daikin NEOFLON EP-541 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Compressive Strength 11.0 MPa
1600 psi
@ 0.2% Offset; ASTM D695
Technetics Group Texolon™ 8534 PTFE  (Unverified Data**)
PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectric ConstantHigh Volume and Surface ResistivityFlame ResistanceApp..
Compressive Strength 11.0 MPa
1600 psi
@ 1.0% Strain; ASTM D695
Technetics Group Texolon™ 8534 PTFE  (Unverified Data**)
PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surface EnergyLow Dielectric ConstantHigh Volume and Surface ResistivityFlame ResistanceApp..
Copyright © lookpolymers.com All Rights Reserved