Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 105 MPa | 15200 psi | Type B, 5mm/min; ISO 604:2002 |
Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled For applications requiring higher compressive strength the NYLUBE GF masterbatch incorporates hollow glass ovule, designed to float and evenly distribute through the polymerising polymer. The glass .. |
|||
Compressive Strength | 105 MPa | 15200 psi | |
Poco Graphite CZR Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Compressive Strength | 105 MPa | 15300 psi | 10% Def.; ASTM D695 |
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet) Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. .. |
|||
Compressive Strength | 105 MPa | 15200 psi | |
Resin Technology Group KONA 870FT-FR Fire Retardant Epoxy Casting System Mix ratio 100 to 4 by weight.KONA 870 FTFR with HARDENER #9 is a versatile epoxy casting system that exhibits unusually high thermal conductivity and low thermal expansion. It is recommended for ele.. |
|||
Compressive Strength | 105 MPa | 15200 psi | Sample Type B, 5 mm/min; ISO 604:2002 |
Global EPP PA 6C MOLY Cast Polyamide 6 + MoS2 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Compressive Strength | 105 MPa | 15300 psi | 10% strain; ASTM D695 |
Saint-Gobain Meldin® 7021 Direct Formed Graphite Filled Polyimide Finished parts and basic shapes made from 15% by weight graphite filled polyimide material for applications high wear resistance, good thermal oxidative stability, and high temperature resistance. .. |
|||
Compressive Strength | 105 MPa | 15200 psi | Absolute Drying; ASTM-D695 |
Toyobo GLAMIDE® T-777-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Compressive Strength | 105 MPa | 15200 psi | ASTM D695 |
Sumitomo Bakelite North America FM 3000 Cellulose Reinforced Phenolic Novolac FM 3000 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear. Information supplied by Sumitomo Bak North America... |