Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 30.0 - 50.0 MPa | 4350 - 7250 psi | ISO 527 |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Tensile Strength | 30.0 - 50.0 MPa | 4350 - 7250 psi | ISO 527 |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Tensile Strength | 40.0 - 50.0 MPa | 5800 - 7250 psi | Compression; ISO 527 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Tensile Strength | 40.0 - 50.0 MPa | 5800 - 7250 psi | Injection; ISO 527 |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Tensile Strength | 38.0 - 50.0 MPa | 5510 - 7250 psi | DIN 53455 |
Isoflon PVDF Polyvinyl Dichloride Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Strength | 45.0 - 50.0 MPa | 6530 - 7250 psi | ASTM D638 |
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |
|||
Tensile Strength | 40.0 - 50.0 MPa | 5800 - 7250 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit.. |
|||
Tensile Strength | 30.0 - 50.0 MPa | 4350 - 7250 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot.. |
|||
Tensile Strength | 30.0 - 50.0 MPa | 4350 - 7250 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR L 4305 Bulk Molding Compound UL-licensed. Anchor wave-isolation.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prote.. |
|||
Tensile Strength | 40.0 - 50.0 MPa | 5800 - 7250 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr.. |