Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 4.00 MPa @Strain 100 % |
580 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3900 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 4.00 MPa | 580 psi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.130 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli.. |
|||
Tensile Strength | 4.00 MPa | 580 psi | |
Momentive Performance Materials Siloprenâ„¢ Electro 242-0 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tensile Strength | 4.00 MPa | 580 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/03 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tensile Strength | 4.00 MPa | 580 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2530 Liquid Silicone Rubber - Textile Coating This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 4.00 MPa | 580 psi | ISO 527 |
Fainplast Compounds Hax™ HFC 0108/4 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:Bedding, designed to meet BS 7846Information provided by Fainplast Compounds |
|||
Tensile Strength | 4.00 MPa @Strain 20.0 % |
580 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan 690 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 4.00 MPa @Strain 300 % |
580 psi @Strain 300 % |
ISO 37 |
BASF Elastollan C 65 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 4.00 MPa | 580 psi | ASTM D 638 |
API Megol AM DP2392/32 SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |
|||
Tensile Strength | 4.00 MPa @Strain 20.0 % |
580 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan 1185 A WM TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 4.00 MPa @Strain 100 % |
580 psi @Strain 100 % |
ISO 37 |
BASF Elastollan B 85 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 4.00 MPa | 580 psi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ LF 6150 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |